Rechargeable zinc ion battery based on sol-gel transition electrolytes

sol-gel-transition-electrolye
Schematic illustration of the thermoresponsive Zn/α-MnO2 batteries with reversible sol-gel transition electrolye. Credit: ©Science China Press

The thermal runaway issue has been a longstanding obstacle impeding the development of high-energy-density, high-power delivery batteries. These batteries would generate a lot of heat in ultrafast charge/discharge process or hazardous conditions, such as overcharging and short-circuits. To dissipate the heat accumulated in the batteries, physical safety designs such as fused disconnect switches, extinguishing agents, and shutdown current collectors have been employed.

However, these approaches only provide one-time protection. There is no provision for these strategies to spontaneously restore the original working condition of batteries once the temperature is cooled down. Therefore, intelligent and active internal safety strategies are required for fabricating smart batteries with dynamic electrochemical performance and self-adaptive response to temperature.

Reversible sol-gel transition hydrogels have received abundant research interest owing to their smart response to ambient temperature. They are normally in flowing liquid state at or below room temperature and can transform into stationary gels when heated above a critical temperature. Moreover, this transition can be reversed after cooling down, displaying interesting temperature-dependent properties. Sol-gel transition polymers may potentially be good candidates for designing advanced batteries with intelligent thermal responsibility.

Recently, a research team led by Prof. Chunyi Zhi from City University of Hong Kong has successfully synthesized a temperature-sensitive sol-gel transition electrolyte comprising proton-incorporated poly(N-isopropylacrylamide-co-acrylic acid) (PNA). They incorporated it into a rechargeable Zn/α-MnO2 battery system. After heating above the low critical temperature, a gelation process occurs in the PNA sol-gel electrolyte and significantly inhibits the migration of zinc ions, leading to a decreased specific capacity and an increased internal resistance of the battery, thus shutting down the battery.